Carbon equivalent (CET): 0.24 [-]

Quick Comparison

Unclassified Low Alloy Steel

DI-MC 355 B (EN S355M)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DI-MC 355 T (EN S355ML)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

EN 10028-5 Grade P420MHTL2

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-5 Grade P420K4

Suministrada por:

1 proveedor Matmatch