Carbon equivalent (CET): 0.29 [-]

Quick Comparison

Unclassified Low Alloy Steel

Quend 700

Suministrada por:

NLMK Europe

Acero inoxidable martensítico

Quard 400

Suministrada por:

NLMK Europe

Unclassified Low Alloy Steel

DI-MC 500 B (EN S500M)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DI-MC 500 T (EN S500ML)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DI-MC 550 B

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DI-MC 550 T

Suministrada por:

Dillinger