Coefficient of friction: 0.21 [-]

Quick Comparison

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RL004

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KAL22

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DL003

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ LUBRICOMP™ Compound OL004

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KA000M

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound RX05497

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DL0049EF

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DL0039EF

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound NXCY620

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL003LH

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RL4040HSUV

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RP004S

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL001

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DX00467H

Suministrada por:

Sabic

Éter de polifenileno (PPE)

LNP™ LUBRILOY™ Compound Z20001

Suministrada por:

Sabic

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QP004

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DP001E

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KX06415

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KP004L

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRILOY™ Compound D20001 - Asia

Suministrada por:

Sabic
Página 1 de 4