Coefficient of friction, kinetic: 0.29 [-]

Quick Comparison

Poliéter éter cetona (PEEK)

LNP™ LUBRICOMP™ Compound LL003XX1

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRILOY™ Compound D20001 - Americas

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL004U

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL004 - Americas

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL004 - Asia

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL004 - Europe

Suministrada por:

Sabic