Coefficient of friction, static: 0.13 [-]

Quick Comparison

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL003LH

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RP004SZ

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL004L

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRILOY™ Compound D20009 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRILOY™ Compound D20009 - Americas

Suministrada por:

Sabic