Wrought Copper Brass Yellow Brass
EN 12163 Grade CuZn36 R370Bronce fosforado
EN 12166 Grade CuSn8 R550Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn37 R370Wrought Copper Pure / Low Alloyed Copper
EN 12163 Grade CuZr R280Wrought Copper Pure / Low Alloyed Copper
EN 12166 Grade CuZr R280Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R540Wrought Copper High Copper Alloy
EN 12163 Grade CuCr1Zr R370Wrought Copper High Copper Alloy
EN 12167 Grade CuCr1Zr R370Bronce fosforado
EN 12166 Grade CuSn8 R420Leaded Brass
EN 12163 Grade CuZn32Pb2AsFeSi R430Wrought Copper Nickel Grade
EN 12163 Grade CuNi30Mn1Fe R420