Acero bajo en carbono
ASTM A920 Grade 15V24 Class 520, Hot-WroughtChromium Molybdenum Steel
ASTM A920 Grade 10V40 Class 520, Hot-WroughtChromium Molybdenum Steel
ASTM A920 Grade 10V45 Class 520, Hot-WroughtMolybdenum Steel
ASTM A920 Grade 11V37 Class 520, Hot-WroughtMolybdenum Steel
ASTM A920 Grade 11V41 Class 520, Hot-WroughtMolybdenum Steel
ASTM A920 Grade 15V41 Class 520, Hot-WroughtUnclassified Carbon Steel
ASTM A615 Grade 520 Designation No. 10