Heat deflection temperature, 1.80 MPa: 181 °C

Quick Comparison

Polisulfona (PSU)

LNP™ LUBRICOMP™ Compound GFL36L

Suministrada por:

Sabic

Polyamide 612 (PA612)

LNP™ THERMOCOMP™ Compound IF003

Suministrada por:

Sabic

Polyamide 6 (PA6)

LNP™ STAT-LOY™ Compound PF303 - Asia

Suministrada por:

Sabic