Heat deflection temperature, 8.0 MPa: 140 °C

Quick Comparison

Polyamide 6T (PA6T)

Polyphthalamide (PPA) HT00 GFR 30 BK Q1D001

Suministrada por:

EPSAN

Polyamide 6T (PA6T)

Polyphthalamide (PPA) HT00 GFR 35 BK Q1D501

Suministrada por:

EPSAN