Impact strength, Izod notched, ASTM: 103 J/m

Quick Comparison

Policarbonato (PC)

LEXAN™ Copolymer CFR9111 - Europe

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound RE007

Suministrada por:

Sabic

Polyamide 612 (PA612)

LNP™ LUBRICOMP™ Compound IFL36L

Suministrada por:

Sabic

Poliéter éter cetona (PEEK)

LNP™ LUBRICOMP™ Compound LFL36E

Suministrada por:

Sabic

Polipropileno

LNP™ THERMOCOMP™ Compound MX00709

Suministrada por:

Sabic