Impact strength, Izod unnotched, ASTM: 1612 J/m

Quick Comparison

Policarbonato (PC)

LNP™ LUBRILOY™ Compound D20001 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRILOY™ Compound D20001 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRILOY™ Compound D20001 - Americas

Suministrada por:

Sabic