Impact strength, Izod unnotched, ASTM: 464 J/m

Quick Comparison

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DBL349E

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ STAT-KON™ Compound DE0069F - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ STAT-KON™ Compound DE0069F - Asia

Suministrada por:

Sabic