Impact strength, Izod unnotched, ASTM: 496 J/m

Quick Comparison

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF002

Suministrada por:

Sabic

Éter de polifenileno (PPE)

LNP™ LUBRICOMP™ Compound ZP001XXP - Asia

Suministrada por:

Sabic