Instrumented Impact, Total Energy: 76 J

Quick Comparison

Policarbonato (PC)

LEXAN™ Copolymer HFD1232 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HFD1232 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HFD1232 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HFD1212 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HFD1212 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HFD1212 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer FXD1414T - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer FXD1414T - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer FXD1414T - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer SLX1432 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer SLX1432 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer SLX1432 - Asia

Suministrada por:

Sabic