Plane-Strain Fracture Toughnes: 10.1 MPa·√m

Quick Comparison

Cobalt Matrix Composite

CTF08M (cemented carbide)

Suministrada por:

CERATIZIT

Cobalt Matrix Composite

KCR10 (cemented carbide)

Suministrada por:

CERATIZIT

Hierro fundido

DIN 1691 Grade GG-15