Cobalt Matrix Composite

CTU17R (cemented carbide)

Suministrada por:

CERATIZIT

Cobalt Matrix Composite

CTF08E (cemented carbide)

Suministrada por:

CERATIZIT

Cobalt Matrix Composite

CTF24T (cemented carbide)

Suministrada por:

CERATIZIT

Cobalt Matrix Composite

CTF28T (cemented carbide)

Suministrada por:

CERATIZIT

Óxido de circonio

Zirconia Mg-PSZ (KZM)

Suministrada por:

Nanoker

Óxido de aluminio

Electroconductive Alumina Composite (KA-EDM)

Suministrada por:

Nanoker

Óxido de aluminio

Alumina SiCw

Suministrada por:

FCT Ingenieurkeramik

Óxido de circonio

ZTA (ZO-AT)

Suministrada por: