Acero bajo en carbono
DIN 1652-3 Grade C15 cold drawnAcero bajo en carbono
EN 10277-2 Grade C15 cold drawnAcero bajo en carbono
EN 10277-2 Grade C15 as rolled and turned (+SH)Acero inoxidable austenítico
EN 10095 Grade X15CrNiSi20-12 solution annealed (+AT)Acero inoxidable austenítico
SEW 470 Grade X15CrNiSi20-12 solution annealed (+AT)Acero bajo en carbono
DIN 17210 Grade C15 soft annealed (+A)