Resistencia al cizallamiento: 526 MPa

Quick Comparison

Acero bajo en carbono

ASTM A203 Grade F Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Wrought Copper Bronze Aluminium Bronze

AMPCO® M4 Forged plates

Suministrada por: