Resistencia al cizallamiento: 585.1 MPa

Quick Comparison

Unclassified Low Alloy Steel

EN 10028-6 Grade P460QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P460QL2 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch