Yield strength Rp0.05: 720 MPa

Quick Comparison

Wrought Copper Nickel Grade

ASTM B740 Grade C72650 TM02

Wrought Copper Nickel Grade

ASTM B740 Grade C72650 TM04

Wrought Copper Nickel Grade

ASTM B740 Grade C72650 TM06

Wrought Copper Nickel Grade

ASTM B740 Grade C72900 TM02

Wrought Copper Nickel Grade

ASTM B740 Grade C72900 TM04

Wrought Copper Nickel Grade

ASTM B740 Grade C72650 TS01

Wrought Copper Nickel Grade

ASTM B740 Grade C72650 TS02

Wrought Copper Nickel Grade

ASTM B740 Grade C72700 TD08

Wrought Copper Nickel Grade

ASTM B740 Grade C72700 TS01

Wrought Copper Nickel Grade

ASTM B740 Grade C72700 TS02

Wrought Copper Nickel Grade

ASTM B740 Grade C72900 TX00

Wrought Copper Nickel Grade

ASTM B740 Grade C72700 TD12

Wrought Copper Nickel Grade

ASTM B740 Grade C72900 TD04

Wrought Copper Nickel Grade

ASTM B740 Grade C72900 TD08