Límite elástico Rp0.5: 90 MPa

Quick Comparison

Copper Bismuth Alloy

ASTM B584 Grade C89844

Copper Bismuth Alloy

ASTM B584 Grade C89844

Wrought Copper Nickel Grade

ASTM B466 Grade C70600 O60

Leaded Tin Bronze

ASTM B505 Grade C93500

Leaded Tin Bronze

ASTM B505 Grade C93700