Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiN18-10 solution annealed (+AT)Acero inoxidable austenítico
JIS G4303 Grade SUS304LN solution treatedAcero inoxidable austenítico
ASTM A240 Grade 304LN Heat-TreatedAcero inoxidable austenítico
JIS G4304 Grade SUS304LN solution treatedAcero inoxidable austenítico
JIS G4305 Grade SUS304LN solution treatedAcero inoxidable austenítico
ASTM A666 Grade 304LN AnnealedAcero inoxidable austenítico
ASTM A276 Grade 304LN Annealed; Hot-FinishedAcero inoxidable austenítico
ASTM A479 Grade 304LN AnnealedAcero inoxidable austenítico
ASTM A988 Grade S30453Acero inoxidable austenítico
ASTM A403 Grade S30453 Heat-TreatedAcero inoxidable austenítico
ASTM A666 Grade 304LN 1/4 HardAcero inoxidable austenítico
ASTM A666 Grade 304LN 1/8 HardAcero inoxidable austenítico
ASTM A666 Grade 304LN 1/16 HardAcero inoxidable austenítico
ASTM A666 Grade 304LN 1/2 HardAcero inoxidable austenítico
AISI 304LN 1/16-HardAcero inoxidable austenítico
AISI 304LN 1/8-HardAcero inoxidable austenítico
AISI 304LN AnnealedAcero inoxidable austenítico
AISI 304LN Quarter-HardAcero inoxidable austenítico
AISI 304LN Half-HardAcero inoxidable austenítico
SAE J405 Grade 304LN