Acero inoxidable austenítico
JIS G4303 Grade SUSXM15J1 solution treatedAcero inoxidable austenítico
ASTM A213 Grade XM-15 Heat-TreatedAcero inoxidable austenítico
JIS G4304 Grade SUSXM15J1 solution treatedAcero inoxidable austenítico
JIS G4305 Grade SUSXM15J1 solution treatedAcero inoxidable austenítico
ASTM A240 Grade XM-15 Heat-TreatedAcero inoxidable austenítico
SAE J405 Grade XM-15