Acero de alto carbono
EN 10250-2 Grade C60 normalized and tempered (+NT)Acero de alto carbono
EN 10083-2 Grade C60 quenched and tempered (+QT)Acero de alto carbono
EN 10083-2 Grade C60 quenched and tempered (+QT)Acero de alto carbono
EN 10083-2 Grade C60 normalized or normalized formed (+N)Acero de alto carbono
EN 10277-2 Grade C60 cold drawnAcero de alto carbono
EN 10083-2 Grade C60 normalized or normalized formed (+N)Acero de alto carbono
EN 10277-2 Grade C60 as rolled and turned (+SH)Acero de alto carbono
AISI 1060 Annealed And Cold DrawnAcero de alto carbono
AISI 1060 Hot RolledAcero de alto carbono
AISI 1060 Spheroidized And Cold DrawnAcero de alto carbono
JIS G4802 Grade S60C annealedAcero de alto carbono
JIS G4802 Grade S60C as cold reducedAcero de alto carbono
JIS G4802 Grade S60C austemperedAcero de alto carbono
JIS G4802 Grade S60C quenched and temperedAcero de alto carbono
JIS G4802 Grade S65C annealedAcero de alto carbono
JIS G4802 Grade S65C as cold reducedAcero de alto carbono
JIS G3311 Grade S60CM annealedAcero de alto carbono
JIS G3311 Grade S60CM cold-rolled