Chromium Steel
EN 10297-1 Grade 41Cr4 quenched and tempered (+QT)Chromium Steel
EN 10263-4 Grade 41Cr4 quenched and tempered (+QT)Chromium Steel
EN 10277-5 Grade 41Cr4 cold drawnChromium Steel
EN 10263-4 Grade 41Cr4 cold drawn, annealed to achieve spheroidized carbides and slightly skin passedChromium Steel
EN 10083-1 Grade 41Cr4 surface hardenedChromium Steel
EN 10083-1 Grade 41CrS4 surface hardenedChromium Steel
ASTM A752 Grade 5140 AnnealedChromium Steel
JIS G3311 Grade SCr440M annealedChromium Steel
JIS G3311 Grade SCr440M cold-rolledChromium Steel
JIS G4052 Grade SCr440HChromium Steel
JIS G4104 Grade SCr440Chromium Steel
SAE J404 Grade 5140Chromium Steel
ASTM A29 Grade 5140Chromium Steel
SAE J1268 Grade 5140H