AISI 429

Quick Comparison

Acero inoxidable ferrítico

JIS G4304 Grade SUS429 annealed

Acero inoxidable ferrítico

JIS G4305 Grade SUS429 annealed

Acero inoxidable ferrítico

ASTM A182 Grade F429 Annealed

Acero inoxidable ferrítico

ASTM A240 Grade 429 Heat-Treated

Acero inoxidable ferrítico

ASTM A268 Grade TP429 Reheated

Acero inoxidable ferrítico

ASTM A473 Grade 429 Annealed

Acero inoxidable ferrítico

ASTM A511 Grade MT429 Annealed

Acero inoxidable ferrítico

ASTM A554 Grade MT429

Acero inoxidable ferrítico

ASTM A815 Grade S42900 Heat-Treated

Acero inoxidable ferrítico

ASTM A493 Grade 429 Lightly Drafted

Acero inoxidable ferrítico

ASTM A493 Grade 429 As-Annealed

Acero inoxidable ferrítico

SAE J405 Grade 429