Medium Carbon Steel
EN 10087 Grade 46S20 quenched and tempered (+QT)Medium Carbon Steel
EN 10277-3 Grade 46S20 cold drawn and quenched and tempered (+C+QT)Medium Carbon Steel
EN 10277-3 Grade 46S20 cold drawnMedium Carbon Steel
EN 10277-3 Grade 46S20 quenched and tempered and cold drawn (+QT+C)Medium Carbon Steel
EN 10087 Grade 46S20 untreatedMedium Carbon Steel
EN 10277-3 Grade 46S20 as rolled and turned (+SH)