Medium Carbon Steel
EN 10083-2 Grade C35E quenched and tempered (+QT)Medium Carbon Steel
EN 10250-2 Grade C35E normalized and tempered (+NT)Medium Carbon Steel
EN 10250-2 Grade C35E normalized or normalized formed (+N)Medium Carbon Steel
EN 10083-2 Grade C35E quenched and tempered (+QT)Medium Carbon Steel
EN 10277-5 Grade Ck35 cold drawn or turned and quenched and temperedMedium Carbon Steel
EN 10083-1 Grade C30E quenched and tempered (+QT)Medium Carbon Steel
EN 10083-1 Grade C30R quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C30 quenched and tempered (+QT)Medium Carbon Steel
EN 10269 Grade C35E quenched and tempered (+QT)Medium Carbon Steel
EN 10132-3 Grade C35E soft annealed or soft annealed and skin passed (+A or +A+LC)Medium Carbon Steel
EN 10083-2 Grade C35E normalized or normalized formed (+N)Medium Carbon Steel
EN 10277-5 Grade Ck35 cold drawnMedium Carbon Steel
EN 10277-5 Grade Ck35 cold drawn or turned and normalizedMedium Carbon Steel
EN 10269 Grade C35E normalized or normalized formed (+N)Medium Carbon Steel
EN 10277-5 Grade C35E quenched and tempered and cold drawn (+QT+C)Medium Carbon Steel
EN 10277-5 Grade C35E cold drawn and quenched and tempered (+C+QT)Medium Carbon Steel
EN 10277-5 Grade C35E cold drawnMedium Carbon Steel
EN 10297-1 Grade Ck35 quenched and tempered (+QT)Medium Carbon Steel
EN 10277-5 Grade C35E as rolled and turned (+SH)Medium Carbon Steel
EN 10297-1 Grade Ck35 normalized or normalized formed (+N)