Chromium Steel
EN 10263-4 Grade 38Cr2 quenched and tempered (+QT)Chromium Steel
DIN 17200 Grade 38Cr2 treated for cold shearing (+S)Chromium Steel
EN 10083-1 Grade 38CrS2 treated for cold shearing (+S)Chromium Steel
EN 10277-5 Grade 38Cr2 cold drawnChromium Steel
EN 10277-5 Grade 38CrS2 cold drawn