Acero de alto carbono
EN 10297-1 Grade C60Pb normalized or normalized formed (+N)Cast Copper Brass Yellow Brass
SIS 145256 Grade 5256Cast Copper Brass Yellow Brass
DIN 1709 Grade 2.0590.03Cast Copper Brass Yellow Brass
DIN 17656 Grade 2.0600Cast Copper Brass Yellow Brass
NP 1566 Grade CC764SCast Copper Brass Yellow Brass
VSM 10810-2 Grade CC764SCast Copper Brass Yellow Brass
DIN 17656 Grade CB764SCast Copper Brass Yellow Brass
ISO 1338 Grade CuZn35AlFeMnCast Copper Brass Yellow Brass
SFS 2205 Grade CuZn35AlFeMnCast Copper Brass Yellow Brass
NS 16565 Grade CuZn35AlFeMnCast Copper Brass Yellow Brass
DIN 1709 Grade CC764SCast Copper Brass Yellow Brass
EN 1982 Grade CC764S