Wrought Copper Bronze Aluminium Bronze
EN 12451 Grade CuAl5As O60Wrought Copper Bronze Aluminium Bronze
ASTM B111 Grade C60800 O61Wrought Copper Bronze Aluminium Bronze
ASTM B395 Grade C60800 O61Copper Silver Zinc Alloy
CEN/TS 13388 Grade 42 3042Copper Silver Zinc Alloy
GOST 18175 Grade BrA5Copper Silver Zinc Alloy
MSZ 711-1 Grade Albz 5Wrought Copper Bronze Aluminium Bronze
ISO 428 Grade CuAl5Copper Silver Zinc Alloy
AFNOR NF A 51-113 Grade CuAl6Copper Silver Zinc Alloy
SN 211605 Grade CuAl5Wrought Copper Bronze Aluminium Bronze
CEN/TS 13388 Grade CuAl5Wrought Copper Bronze Aluminium Bronze
DIN 17665 Grade CW300GWrought Copper Bronze Aluminium Bronze
NP 3638 Grade CW300GWrought Copper Bronze Aluminium Bronze
PN/H 87051 Grade CW300GWrought Copper Bronze Aluminium Bronze
ÖNORM M 3409 Grade CW300GWrought Copper Bronze Aluminium Bronze
UNI 7989-1 Grade CW300GWrought Copper Bronze Aluminium Bronze
CEN/TS 13388 Grade CW300GCopper Silver Zinc Alloy
GB 5233 Grade QAl5Wrought Copper Bronze Aluminium Bronze
ASTM C60800Copper Silver Zinc Alloy
ASTM C60600