DIN GS-42CrMo4

Quick Comparison

Chromium Molybdenum Steel

EN 10277-5 Grade 42CrMo4 cold drawn

Chromium Molybdenum Steel

JIS G4108 Grade SNB22-4

Chromium Molybdenum Steel

JIS G4108 Grade SNB22-1

Chromium Molybdenum Steel

JIS G4108 Grade SNB22-2

Chromium Molybdenum Steel

JIS G4108 Grade SNB22-3
Página 1 de 2