DIN X6CrNiMo17-13

Quick Comparison

Acero inoxidable austenítico

JIS G3463 Grade SUS316HTB

Acero inoxidable austenítico

JIS G3459 Grade SUS316HTP

Acero inoxidable austenítico

JIS G3467 Grade SUS316HTF

Acero inoxidable austenítico

ASTM A403 Grade S31609 Heat-Treated

Acero inoxidable austenítico

JIS G3214 Grade SUSF316H

Acero inoxidable austenítico

Sandvik 8R61

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Acero inoxidable austenítico

SAE J405 Grade 316H