GOST 35G2

Quick Comparison

Medium Carbon Steel

AISI 1541 Cold Drawn

Medium Carbon Steel

AISI 1541 Hot Rolled

Medium Carbon Steel

JIS G5111 Grade SCMn3A

Medium Carbon Steel

JIS G4106 Grade SMn438

Medium Carbon Steel

SAE J403 Grade 1541

Manganese Steel

SAE J1268 Grade 1335H

Manganese Steel

SAE J404 Grade 1335

Unclassified Carbon Steel

JIS G3539 Grade SWCH41K