JIS BC In 2

Quick Comparison

Leaded Tin Bronze

ASTM B505 Grade C92300

Leaded Tin Bronze

ASTM B505 Grade C92300

Leaded Tin Bronze

ASTM B584 Grade C92300

Leaded Tin Bronze

GOST 613 Grade BrO8Z4