JIS LBCIn2

Quick Comparison

Leaded Tin Bronze

CEN/TS 13388 Grade 423121

Leaded Tin Bronze

AS/NZS 1565 Grade C92710

Leaded Tin Bronze

MSZ 8579 Grade CuPb5Sn10

Leaded Tin Bronze

JIS H2207 Grade LBC In 2

Leaded Tin Bronze

JIS H5115 Grade LBC2