Acero inoxidable austenítico
ASTM A276 Grade XM-10 Annealed; Hot-Finished or Cold-FinishedAcero inoxidable austenítico
ASTM A473 Grade XM-10 AnnealedAcero inoxidable austenítico
ASTM A580 Grade XM-10 Condition A; Cold finishedAcero inoxidable austenítico
ASTM A312 Grade TPXM-10Acero inoxidable austenítico
ASTM A813 Grade TPXM-10 Heat-Treated