ASTM B188

Quick Comparison

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10300 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10500 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C11000 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C11600 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C12000 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10100 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10200 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10400 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10700 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C11300 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C11400 O60

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10200 H80

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10300 H80

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10400 H80

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C10500 H80

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C11000 H80

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C11300 H80

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C11400 H80

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C11600 H80

Wrought Copper Pure / Low Alloyed Copper

ASTM B188 Grade C12000 H80
Página 1 de 2