Wrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn30AsOther Copper Zinc Alloy
ISO 426-1 Grade CuZn31SiWrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn33Other Copper Zinc Alloy
ISO 426-1 Grade CuZn20Al2Wrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn40Wrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn10Wrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn15Wrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn20Wrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn37Tin Brass
ISO 426-1 Grade CuZn37Sn1Pb1Tin Brass
ISO 426-1 Grade CuZn28Sn1Wrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn30Tin Brass
ISO 426-1 Grade CuZn38Sn1Wrought Copper Brass Yellow Brass
ISO 426-1 Grade CuZn5Wrought Copper Brass
ISO 426-1 Grade CuZn37Mn3Al2Si