Acero bajo en carbono
ASTM A320 Grade L1 Quenched and TemperedAcero inoxidable austenítico
ASTM A320 Grade B8MLN Class 1, Carbide Solution TreatedAcero inoxidable austenítico
ASTM A320 Grade B8MLNA Class 1A, Carbide Solution Treated in the Finished ConditionAcero inoxidable austenítico
ASTM A320 Grade B8P Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable austenítico
ASTM A320 Grade B8T Class 1, Carbide Solution TreatedAcero inoxidable austenítico
ASTM A320 Grade B8T Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable austenítico
ASTM A320 Grade B8A Class 1A, Carbide Solution Treated in the Finished ConditionAcero inoxidable austenítico
ASTM A320 Grade B8C Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable austenítico
ASTM A320 Grade B8F Class 1, Carbide Solution TreatedAcero inoxidable austenítico
ASTM A320 Grade B8F Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable austenítico
ASTM A320 Grade B8LN Class 1, Carbide Solution TreatedAcero inoxidable austenítico
ASTM A320 Grade B8M Class 1, Carbide Solution TreatedAcero inoxidable austenítico
ASTM A320 Grade B8 Class 1, Carbide Solution TreatedAcero inoxidable austenítico
ASTM A320 Grade B8C Class 1, Carbide Solution TreatedAcero inoxidable austenítico
ASTM A320 Grade B8P Class 1, Carbide Solution TreatedAcero inoxidable austenítico
ASTM A320 Grade B8PA Class 1A, Carbide Solution Treated in the Finished ConditionAcero inoxidable austenítico
ASTM A320 Grade B8TA Class 1A, Carbide Solution Treated in the Finished ConditionAcero inoxidable austenítico
ASTM A320 Grade B8CA Class 1A, Carbide Solution Treated in the Finished ConditionAcero inoxidable austenítico
ASTM A320 Grade B8FA Class 1A, Carbide Solution Treated in the Finished ConditionAcero inoxidable austenítico
ASTM A320 Grade B8LNA Class 1A, Carbide Solution Treated in the Finished Condition