Aircraft Aluminium Grades

Aluminium is one of the most widely used metals in the world, only second to iron. It is also the most abundant in the earth’s crust constituting about 8% of it by mass. As one of the most versatile metals, it can be combined with other metals to improve their properties and its own properties, as well. In its pure form, aluminium has virtually no practical use and has to be alloyed with other metals for application. Currently the largest producer of the primary aluminium ore, bauxite, in the world is Australia and the largest producer of aluminium is China, producing a whopping 32.6 million metric tonnes [1], almost ten times more than the next largest producer, Russia, and accounting for more than half of the world’s production.

Aluminium has three excellent properties in particular that make it so useful in the aviation industry; high strength to weight ratio, ductility and resistance to corrosion. It is also non-magnetic. There is a wide range of variations in the compositions of aluminium alloys for specific functions in an aircraft.

In this article, you will learn about:

  • The history of aluminium in aircraft
  • Aluminium material properties
  • Aluminium grades used in aircraft
  • Future utilisation of aluminium in future spacecraft

aluminium aircraft 1.jpg

History of aluminium in aircraft

The history of aluminium in aircraft dates back to the beginning of flight itself. On December 17, 1903, the Wright Brothers famously became the first people to fly in an aeroplane. To achieve this feat, they had to create a special engine made of aluminium instead of steel as was the norm at the time. The reason was to make the engine light enough to take flight. This was the beginning of aluminium’s use in aviation.

By the First World War, aluminium began to also constitute the body of airplanes, replacing materials such as wood and canvas. The first fully metal plane, the Junkers J 1, was designed by German aircraft designer Hugo Junkers in 1915, with aluminium alloy tubing in its internal structure [2]. The time between World War I and World War II came to be known as the golden era in aviation during which the use of aluminium alloys became more sophisticated as designs were emerging at a faster rate [3]. This new found application for aluminium caused the demand to soar and consequently aluminium production to rise.

In contemporary times, aluminium’s use in aviation has taken on more sophistication, but the bottom line advantage has remained the same, namely; lightweight, strength and resistance to corrosion. Indeed, the very popular Boeing 737 consists of 80% aluminium. Virtually no part of a plane that can be substituted with aluminium is spared in the modern era with parts such as the fuselage, the wings, the doors, the floors, and the seats, now all being made of aluminium.

Table 1. Application of Aluminium alloys in Aircraft Components (adapted from [4])

Component

Material

Alloy elements

Properties

Front legs of seat

Al 2017, Al 2024

 

Copper, Magnesium

Good machining, high strength, high fatigue strength, corrosion resistance

Wing leading edge

Al 2024

Seat ejectors

Al 2024

Backrests and armrests

Al 6xxx

Magnesium, Silicon

High strength, good formability and weldability, corrosion resistance

Fuselage skins, stringers and bulkheads

Al 6013, Al 6050, Al 7050, Al 7079

Wing skins, panels and covers

Al 7075

 

Zinc, Magnesium, Copper

 

 

Highest strength, high toughness, good formability

Rear legs of seat and seat spreaders

Al 7075

Wing spars, ribs

7055-T77

Wheels and loading gear links

7055-T77

Horizontal and vertical stabilisers

Al 7xxx

Upper and lower wing skins

8090-T86, 2055-T8, 2199-T8E80

 

Lithium, Copper, Magnesium

 

Low density, excellent fatigue and toughness, crack growth resistance

Floor sections of the aircraft

2090-T83, 2090-T62

Sear structure

2090-T83

Supporting members of fuselage structure

8090-T651, 2090-T651

Aluminium material properties

Aluminium is notoriously difficult to extract from its ores due to its high reactivity. However, it takes only 5% of the energy required to extract aluminium from its ores to recycle it. About three-quarters of all the aluminium ever produced is still in use today, which is a testament to its high rate of recyclability. Aluminium in open air reacts with oxygen to form an oxide, but unlike iron, aluminium’s oxide sticks to its surface, thereby protecting it from further corrosion. Alloys of aluminium number in the hundreds as it is very versatile. In the aviation industry, there are very specific requirements which aluminium alloys (or grades) are tailored towards with all of them retaining the most important quality, lightweight. Aluminium's weight is a third that of stainless steel for a given volume but has twice the strength-to-weight ratio of stainless steel. Aluminium loses some of its strength at high temperatures, but under sub-zero temperatures, its strength increases, which is a useful feature in aerospace as aircraft fly at very low-temperature atmosphere.

Table 2. Comparison of Aluminium, Beryllium and Magnesium (adapted from [5])

 

Aluminium

Beryllium

Magnesium

Boiling point

2494oC

2770oC

1107oC

Density

Low

Low

Low

Strength

High

High

High

Toxicity

Non-toxic

Highly toxic

Low toxicity

Flammability

Nil

Flammable

Highly flammable

Integrity at elevated temperatures

Maintains its structure at high temperatures

Relative stability at high temperatures

Obeys a unary phase diagram

Corrosion resistance

High

Medium

Highly corrosive

Reaction with water and acids

Nil

High

High

aluminium aircraft 3.jpg

Aluminium grades in aircraft

Aluminium alloys are designated via a 4 digit numbering system with the first digit representing the alloy group and the other numbers representing the other metals that are present in the alloy. Temper designations are denoted by a prefix such to indicate what type of treatment it has undergone and to what degree. The letters are F, O, H, W, or T to indicate fabrication, annealing, strain hardening, solution heat treatment and heat treatment, respectively [6].

The proportions and constituents of an aluminium alloy determine the specific properties it exhibits. There are literally hundreds of aluminium alloys in use today in different fields of application. For aircraft, below are the most commonly used ones and why they have been chosen for their respective applications [7].

2024-T3

2024-T3 is made up of 4.5% copper, 0.6% manganese and 1.5% magnesium. This is a top tier high strength aluminium alloy and coupled with its fatigue resistance, it is one of the most common aircraft alloys. It doesn’t do well with welding but is a good option for repair works as it has an excellent finish. It is not heat treatable.

6061-T6

6061-T6 is made up of 0.25% copper, 0.6% silicon, 1.0% magnesium and 0.25% chromium. This alloy also has good finishing. In addition to that, it offers good corrosion resistance and is very good for welding. Its strength and workability are comparable to mild steel. It is heat treatable.

3003-H14

3003-H14 contains 1.2% manganese and is the most widely used aluminium alloy. It is very easy to work with as it can be extruded, brazed, machined and welded. It is not heat treatable but can develop increased strength from cold working.

7075-T6

7075-T6 is made up of 1.6% copper, 2.5% magnesium and 5.6% zinc. It is commonly used by aircraft manufacturers to strengthen the structure of the aircraft. It has poor weldability due to its copper content but it has great machinability. It is heat treatable.

5052-H32

5052-H32 is made up of 2.5% magnesium and 0.25% chromium. This alloy offers the highest strength in the non-heatable alloy series and can develop increased strength from cold working. It also has excellent fatigue strength, corrosion resistance and workability which makes it suitable for aviation and marine purposes.

Future utilisation of aluminium in spacecraft

Aluminium is also in use in spacecraft, a field where aluminium’s unique properties would be of even greater importance. Indeed, all spacecraft are primarily made up of aluminium, up to 90%. Aluminium components not only make for spacecraft but also for space stations such as the Skylab and the International Space Station. The Orion spacecraft which is under development with an aluminium-lithium alloy is expected to open up new frontiers in the field of manned space exploration.

Fuentes

[1] "Top 10 Largest Aluminium Producing Countries in the World (2018)", Bizvibe [Online], 2018.

[2] "Quest for Performance: The Evolution of Modern Aircraft", NASA History [Online].

[3] "History of Aluminum in the Aerospace Industry", Metal Supermarkets [Online], 2016.

[4] K. Yashpal et al, "A Review on use of Aluminium Alloys in Aircraft Components", i-manager's Journal on Material Science, 3, 33-38, 2015.

[5] I. Festus & E. Jha, "Why Aluminium is preferred as an aircraft fuselage material: A review", 2017.

[6] S. Koch, "A quick guide to understanding aluminium temper designations", Shapes. [Online], 2018.

[7] "Aircraft Aluminium", Experimental Aircraft Info [Online].

Fun Facts

  • In the early days of aviation, wooden aircraft were the norm as they flourished until WW1, when lightweight aluminium began to take over as a crucial material in aircraft manufacture, superseding wood.
  • During the Golden Age of Aviation, Henry Ford took his company into the airline industry as he used corrugated aluminium to design the 4-AT, an all-metal, three-engine plane that was famously called "The Tin Goose".
  • The infamous Concorde airplane was constructed with an aluminium skin, until it was retired in 2003.