General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.71 g/cm³ Show Supplier Material materials with Densidad of 2.71 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.15 - 0.35 mm Show Supplier Material materials with Espesor of 0.15 - 0.35 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 45 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 45 [-] | according to EN 485-2 |
Elongación A50 | 23.0 °C | 1.5 % Show Supplier Material materials with Elongación A50 of 1.5 % | according to EN 485-2 |
Límite elástico | 23.0 °C | 115 MPa Show Supplier Material materials with Límite elástico of 115 MPa | according to EN 485-2 |
Módulo de cizallamiento | 23.0 °C | 26 GPa Show Supplier Material materials with Módulo de cizallamiento of 26 GPa | |
Módulo elástico | 23.0 °C | 69 GPa Show Supplier Material materials with Módulo elástico of 69 GPa | |
Resistencia a la tracción | 23.0 °C | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | according to EN 485-2 |
Ángulo de flexión a 90° | 23.0 °C | 1 °/t Show Supplier Material materials with Ángulo de flexión a 90° of 1 °/t | according to EN 485-2 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 220 W/(m·K) Show Supplier Material materials with Conductividad térmica of 220 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.82E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.82E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.05 % Show Supplier Material materials with Cobre of 0.05 % |
Cromo | 0.01 % Show Supplier Material materials with Cromo of 0.01 % |
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % |
Magnesio | 0.3 - 0.4 % Show Supplier Material materials with Magnesio of 0.3 - 0.4 % |
Manganeso | 0.05 % Show Supplier Material materials with Manganeso of 0.05 % |
Silicona | 0.25 % Show Supplier Material materials with Silicona of 0.25 % |
Zinc | 0.07 % Show Supplier Material materials with Zinc of 0.07 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Lithography | |
Brazing | Excellent | |
Corrosion properties | Excellent | |
Welding | Excellent | |
Workability | Excellent |