General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Densidad of 2.69 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.2 - 3 mm Show Supplier Material materials with Espesor of 0.2 - 3 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 40 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 40 [-] | according to EN 485-2 |
Elongación A50 | 23.0 °C | 2 % Show Supplier Material materials with Elongación A50 of 2 % | according to EN 485-2 |
Límite elástico | 23.0 °C | 105 MPa Show Supplier Material materials with Límite elástico of 105 MPa | according to EN 485-2 |
Módulo de cizallamiento | 23.0 °C | 26.5 GPa Show Supplier Material materials with Módulo de cizallamiento of 26.5 GPa | |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa | |
Resistencia a la tracción | 23.0 °C | 124 MPa Show Supplier Material materials with Resistencia a la tracción of 124 MPa | according to EN 485-2 |
Ángulo de flexión a 90° | 23.0 °C | 2.5 °/t Show Supplier Material materials with Ángulo de flexión a 90° of 2.5 °/t | according to EN 485-2 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.3E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Conductividad térmica of 138 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 4.9E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 4.9E-8 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Cobre | 0.03 % Show Supplier Material materials with Cobre of 0.03 % | |
Hierro | 0.15 % Show Supplier Material materials with Hierro of 0.15 % | |
Magnesio | 0.02 % Show Supplier Material materials with Magnesio of 0.02 % | |
Manganeso | 0.02 % Show Supplier Material materials with Manganeso of 0.02 % | |
Otro | 0.02 % Show Supplier Material materials with Otro of 0.02 % | Min. |
Silicona | 0.15 % Show Supplier Material materials with Silicona of 0.15 % | |
Zinc | 0.06 % Show Supplier Material materials with Zinc of 0.06 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Cosmetics: Cosmetic pieces; Automotive trim: Interior trim, Windows frame, Marque badges | |
Brazing | Excellent | |
Corrosion properties | Excellent | |
Welding | Excellent | |
Workability | Excellent |