General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Densidad of 2.7 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.3E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 235 W/(m·K) Show Supplier Material materials with Conductividad térmica of 235 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.79E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.79E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.03 % Show Supplier Material materials with Cobre of 0.03 % |
Galio | 0.03 % Show Supplier Material materials with Galio of 0.03 % |
Hierro | 0.12 % Show Supplier Material materials with Hierro of 0.12 % |
Magnesio | 0.02 % Show Supplier Material materials with Magnesio of 0.02 % |
Manganeso | 0.02 % Show Supplier Material materials with Manganeso of 0.02 % |
Otro | 0.01 % Show Supplier Material materials with Otro of 0.01 % |
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % |
Titanio | 0.02 % Show Supplier Material materials with Titanio of 0.02 % |
Vanadio | 0.05 % Show Supplier Material materials with Vanadio of 0.05 % |
Zinc | 0.03 % Show Supplier Material materials with Zinc of 0.03 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Cosmetics: Cosmetic pieces; Automotive trim: Interior trim, Windows frame, Marque badges | |
Corrosion properties | Excellent | |
Welding | Excellent | |
Workability | Excellent |