General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.71 g/cm³ Show Supplier Material materials with Densidad of 2.71 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 218 W/(m·K) Show Supplier Material materials with Conductividad térmica of 218 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 3E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3E-8 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Cobre | 0.05 - 0.2 % Show Supplier Material materials with Cobre of 0.05 - 0.2 % | |
Hierro | 0.95 % Show Supplier Material materials with Hierro of 0.95 % | Si + Fe |
Manganeso | 0.05 % Show Supplier Material materials with Manganeso of 0.05 % | |
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % | |
Silicona | 0.95 % Show Supplier Material materials with Silicona of 0.95 % | Si + Fe |
Zinc | 0.1 % Show Supplier Material materials with Zinc of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Very Good | |
Application areas | Roofing: Foil for bituminous coating; Interiors and ceilings: Decoration; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Heat exchangers: Fins, General applications; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Components: Automotive fins, Heat exchangers | |
Brazing | Excellent | |
Corrosion properties | Very Good | |
Welding | Excellent | |
Workability | Excellent |