General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Densidad of 2.69 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 60 - 400 mm Show Supplier Material materials with Espesor of 60 - 400 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 1 % Show Supplier Material materials with Elongación A50 of 1 % |
Límite elástico | 23.0 °C | 95 - 150 MPa Show Supplier Material materials with Límite elástico of 95 - 150 MPa |
Módulo de cizallamiento | 23.0 °C | 26.5 GPa Show Supplier Material materials with Módulo de cizallamiento of 26.5 GPa |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa |
Resistencia a la tracción | 23.0 °C | 105 - 170 MPa Show Supplier Material materials with Resistencia a la tracción of 105 - 170 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Conductividad térmica of 138 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 4.9E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 4.9E-8 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Cobre | 0.05 % Show Supplier Material materials with Cobre of 0.05 % | |
Hierro | 1 % Show Supplier Material materials with Hierro of 1 % | Si + Fe |
Manganeso | 0.05 % Show Supplier Material materials with Manganeso of 0.05 % | |
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | Si + Fe |
Titanio | 0.05 % Show Supplier Material materials with Titanio of 0.05 % | |
Zinc | 0.1 % Show Supplier Material materials with Zinc of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Very Good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels; Roofing: Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels; Electronic devices: Housing of devices; Heat exchangers: Fins; Cable wrapping: Electric cable wrapping; Insulation; Solar: Solar collectors; Semi-rigid and corrugated: Smooth wall | |
Brazing | Excellent | |
Corrosion properties | Very Good | |
Welding | Excellent | |
Workability | Excellent |