General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Densidad of 2.69 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.2 - 3 mm Show Supplier Material materials with Espesor of 0.2 - 3 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo de cizallamiento | 23.0 °C | 26.5 GPa Show Supplier Material materials with Módulo de cizallamiento of 26.5 GPa |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa |
Ángulo de flexión a 90° | 23.0 °C | 3 °/t Show Supplier Material materials with Ángulo de flexión a 90° of 3 °/t |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Conductividad térmica of 138 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 4.9E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 4.9E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.05 % Show Supplier Material materials with Cobre of 0.05 % |
Cromo | 0.01 % Show Supplier Material materials with Cromo of 0.01 % |
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % |
Manganeso | 0.01 % Show Supplier Material materials with Manganeso of 0.01 % |
Otro | 0.1 % Show Supplier Material materials with Otro of 0.1 % |
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % |
Zinc | 0.05 % Show Supplier Material materials with Zinc of 0.05 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Good (For surface protection only) | |
Application areas | Conductors; rods for the manufacture of aluminium conductor wires. | |
Brazing | Excellent | |
Corrosion properties | Very Good | |
Welding | Very Good | |
Workability | Very Good |