General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.72 g/cm³ Show Supplier Material materials with Densidad of 2.72 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.2 - 2 mm Show Supplier Material materials with Espesor of 0.2 - 2 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 33 - 73 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 33 - 73 [-] |
Elongación A50 | 23.0 °C | 1 % Show Supplier Material materials with Elongación A50 of 1 % |
Límite elástico | 23.0 °C | 45 MPa Show Supplier Material materials with Límite elástico of 45 MPa |
Módulo de cizallamiento | 23.0 °C | 26 GPa Show Supplier Material materials with Módulo de cizallamiento of 26 GPa |
Módulo elástico | 23.0 °C | 69 GPa Show Supplier Material materials with Módulo elástico of 69 GPa |
Resistencia a la tracción | 23.0 °C | 115 - 290 MPa Show Supplier Material materials with Resistencia a la tracción of 115 - 290 MPa |
Ángulo de flexión a 180° | 23.0 °C | 0 °/t Show Supplier Material materials with Ángulo de flexión a 180° of 0 °/t |
Ángulo de flexión a 90° | 23.0 °C | 0 °/t Show Supplier Material materials with Ángulo de flexión a 90° of 0 °/t |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 172 W/(m·K) Show Supplier Material materials with Conductividad térmica of 172 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 3.8E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.8E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.3 % Show Supplier Material materials with Cobre of 0.3 % |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % |
Hierro | 0.7 % Show Supplier Material materials with Hierro of 0.7 % |
Magnesio | 0.2 - 0.6 % Show Supplier Material materials with Magnesio of 0.2 - 0.6 % |
Manganeso | 1 - 1.5 % Show Supplier Material materials with Manganeso of 1 - 1.5 % |
Silicona | 0.6 % Show Supplier Material materials with Silicona of 0.6 % |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Electronic devices: Housing of devices; Insulation; Cosmetics: Cosmetics pieces | |
Brazing | Good | |
Corrosion properties | Good | |
Welding | Good | |
Workability | Good |