General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Densidad of 2.7 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.2 - 3 mm Show Supplier Material materials with Espesor of 0.2 - 3 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 47 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 47 [-] |
Elongación A50 | 23.0 °C | 3 - 5 % Show Supplier Material materials with Elongación A50 of 3 - 5 % |
Límite elástico | 23.0 °C | 110 MPa Show Supplier Material materials with Límite elástico of 110 MPa |
Módulo de cizallamiento | 23.0 °C | 26.5 GPa Show Supplier Material materials with Módulo de cizallamiento of 26.5 GPa |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa |
Resistencia a la tracción | 23.0 °C | 145 - 185 MPa Show Supplier Material materials with Resistencia a la tracción of 145 - 185 MPa |
Ángulo de flexión a 180° | 23.0 °C | 1.5 °/t Show Supplier Material materials with Ángulo de flexión a 180° of 1.5 °/t |
Ángulo de flexión a 90° | 23.0 °C | 1 °/t Show Supplier Material materials with Ángulo de flexión a 90° of 1 °/t |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 200 W/(m·K) Show Supplier Material materials with Conductividad térmica of 200 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 3.3E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.3E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.2 % Show Supplier Material materials with Cobre of 0.2 % |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % |
Hierro | 0.7 % Show Supplier Material materials with Hierro of 0.7 % |
Magnesio | 0.5 - 1.1 % Show Supplier Material materials with Magnesio of 0.5 - 1.1 % |
Manganeso | 0.2 % Show Supplier Material materials with Manganeso of 0.2 % |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent (anodizing quality) | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Anodizing quality; Heat exchangers: Fins, General applications; Cosmetics: Cosmetics pieces; Automotive trim: Interior trim; Components: Automotive fins, Heat exchangers | |
Brazing | Good | |
Corrosion properties | Excellent | |
Welding | Very Good | |
Workability | Very Good |