General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.67 g/cm³ Show Supplier Material materials with Densidad of 2.67 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 125 W/(m·K) Show Supplier Material materials with Conductividad térmica of 125 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 5.7E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.7E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.15 % Show Supplier Material materials with Cobre of 0.15 % |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % |
Hierro | 0.35 % Show Supplier Material materials with Hierro of 0.35 % |
Magnesio | 3 - 4 % Show Supplier Material materials with Magnesio of 3 - 4 % |
Manganeso | 0.2 - 0.5 % Show Supplier Material materials with Manganeso of 0.2 - 0.5 % |
Otro | 0.05 - 0.15 % Show Supplier Material materials with Otro of 0.05 - 0.15 % |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent (anodizing quality) | |
Application areas | Vessels: Pressure; Wind energy: Nacelle coverings, rotor hub, stairs; Food can: Body, Lids; Components: Access hatches, Spoilers, General transportation | |
Corrosion properties | Excellent | |
Welding | Good | |
Workability | Good (in O temper) |